Lembaran, Foil & Strip Baja Tahan Karat 17-7PH
Jan 29, 2026
Tinggalkan pesan



| Standar |
AMS 5528, AMS 5529, AMS 5568, ASTM A666, ASTM A693 |
|---|---|
| Nilai |
0Cr17Ni7Al, 1,4568, 631, S17700, SUS 631 |
| Panjang |
Disesuaikan, Lembar: 1000 mm-3000 mm (39,37-118,11 in) |
| Ketebalan |
Disesuaikan, Foil: 0,01 mm-0,1 mm (0,0004-0,004 inci), Lembar: 0,25 mm-3 mm (0,01-0,12 inci), Strip: 0,1 mm-2 mm (0,004-0,078 inci) |
| Lebar Penuh |
Disesuaikan, Foil: 10 mm-600 mm (0,4-24 inci), Lembaran: 500 mm-1500 mm (19,7-59,06 inci), Strip: 10 mm-500 mm (0,4-19,7 inci) |
| Permukaan Selesai |
2B, 2D, BA, Dilapisi, dll., Pabrik, No.1, No.4 |
| Teknik |
Ditarik Dingin, Digulung Dingin, Digulung Panas |
| Membentuk |
17-7PH Foil, 17-7PH Sheet, 17-7PH Strip, Annealed Sheet, Brushed Sheet, Coated Strip, Coil, Cold Rolled Sheet, Cold-Rolled Foil, Deburred Edge Strip, dll., Etched Foil, Heat Treated Foil, Hot Rolled Sheet, Hot-Rolled Strip, Perforated sheet, Plate, Precision Strip, Tempered Foil |