When selecting stainless steel tubes for heat exchangers, dimensional tolerances play a critical role in system performance, weldability, and fit-up. Two of the most commonly specified ASTM standards are ASTM A213 and ASTM A249. While both are used in high-pressure, high-temperature, and corrosive environments, they differ significantly in manufacturing method and tolerance kontrol .

 

ASTM A213 VS .ASTM A249 Heat Exchanger Tube

ASTM A213 vs . ASTM A249 Tabung penukar panas

Spesifikasi ASTM A213 ASTM A249
Jenis tabung Mulus atau dilas (ditarik dingin) Dilas (dan bekerja dingin jika ditentukan)
Aplikasi Boiler, superheater, penukar panas Penukar panas, kondensor, tabung boiler
Kencangkan toleransi Lebih ketat (terutama untuk OD dan Wall) Kurang ketat, lebih fleksibel
Proses pembuatan Gambar dingin presisi Pengelasan Otomatis + Kerja Dingin
Nilai khas TP304, TP316, TP321, TP347 TP304, TP316, TP304L, TP316L

ASTM A213 vs . ASTM A249 Tabung penukar panas: Toleransi

Spesifikasi Ukuran OD Range Inches Toleransi
O.D. Dinding
Plus Minus Plus Minus
ASTM-A -249 Di bawah 1.000 .004" .004" 10% l0%
Asme-sa -249 1.000 hingga 1.500 .006" .006" 10% 10%
Welded & Cold Work 1.501 hingga 1.999 .008" .008" l0% 10%
Tabung penukar panas 2.000 hingga 2.499 .010" .010" 10% 10%
Dinding rata -rata 2.500 hingga 2.999 .012" .012" 10% 10%
(Lihat Catatan 1) 3.000 hingga 4.000 .015" .015" 10% 10%
  4.001 hingga 5.000 .015" .025" 10% 10%
ASTM-A -213 Di bawah 1.000 .004" .004" 20% 0%
Asme-sa -213 1.000 hingga 1.500 .006" .005" 20% 0%
Dingin jadi mulus 1.501 hingga 1.999 .008" .008" 22% 0%
Tabung penukar panas 2.000 hingga 2.499 .010" .010" 22% 0%
Dinding minimum 2.500 hingga 2.999 .012" .012" 22% 0%
(Lihat Catatan 2 & 3) 3.000 hingga 4.000 .015" .015" 22% 0%
  4.001 hingga 5.000 .015" .025" 22% 0%

Notes (1) juga tersedia di dinding minimum + 18/-0% . (2) Juga tersedia di dinding rata -rata ± 10% (3) juga tersedia panas, lihat spesifikasi untuk toleransi .