Baja Tahan Karat Martensit yang Dapat Dikeraskan: Kelas 4101.4006 di Cina

Apr 13, 2026

Tinggalkan pesan

1.4401 vs 1.4404 Stainless Steel: Chemical Composition304 vs. 316 vs. 310S Stainless Steel Tubes: High-Temperature ResistanceChemical Composition and Properties: What Sets 201 and 304 Apart?Stainless steel of 310s in Gnee steel

Komposisi Kimia

1.4006 BajaEN 10088-3:2005
Unsur Kimia% Hadiah
Karbon (C)0.08 - 0.15
Kromium (Cr)11.50 - 13.50
Silikon (Si)0.0 - 1.00
Mangan (Mn)0.0 - 1.50
Fosfor (P)0.0 - 0.04
Belerang (S)0.0 - 0.02
Nikel (Ni)0.0 - 0.75
Besi (Fe)Keseimbangan

 

Properti

Properti FisikNilai
Kepadatan7,75 gram/cm³
Ekspansi Termal9.9 x 10-6/K
Modulus Elastisitas300 IPK
Konduktivitas Termal24.9 W/m.K
Resistivitas Listrik0.57 x 10-6Ω.m
Batangan - Diameter atau Ketebalan Hingga 160mmEN 10088-3:2005
Properti MekanikNilai
Bukti Stres450 menit MPa
Kekuatan Tarik650 - 850 MPa
Pemanjangan A15 Menit %