Lembaran Baja Tahan Karat 201

Mar 10, 2026

Tinggalkan pesan

UNS S40900 Stainless Steel304L Stainless Steel Coil for Food Packaging310 Stainless Steel Pipe for High-Temperature Flue Gas Transmission

Standar

ASTM A240, EN 10088-2, GB/T 3280

Nilai

1.4372, SUS201, X12CrMnNiN17-7-5, Z12CMN17-07Az

Panjang

2000 mm-6000 mm (78,74-236,22 inci), Disesuaikan

Lebar Penuh

1000 mm-2000 mm (39,37-78,74 inci), Disesuaikan

Ketebalan

0,3 mm-6 mm (0,012-0,24 inci), Disesuaikan

Permukaan Selesai

2B, 8K, BA, dll., HL, No.1, No.4

Teknik

Ditarik Dingin, Digulung Dingin, Digulung Panas

Membentuk

Coil, Cold Rolled Sheet, Embossed Sheets, dll., Flat Plate & Sheet, Hot Rolled Sheet, Perforated Sheets, Plate, Polished Sheets, Strip, Textured Sheets

 

Komposisi Kimia

Elemen Karbon (C) Mangan (Mn) Silikon (Si) Fosfor (P) Belerang (S) Kromium (Cr) Nikel (Ni) Nitrogen (N)
                 
Komposisi (%) 0,15 maks 5.5-7.5 1,0 maks 0,06 maks 0,03 maks 16.0-18.0 3.5-5.5 0,25 maks

Sifat Mekanik

Properti Satuan Metrik Satuan Kekaisaran
     
Kekuatan Tarik 655 – 860 MPa 95 – 125xi
Kekuatan Hasil 450 MPa 65ksi
Kekerasan Vickers 230 – 270 HV 230 – 270 HV
Kekerasan Brinell 200 – 250 HB 200 – 250 HB
Kekerasan Rockwell 50 – 56 HRC 50 – 56 HRC
Pemanjangan 20% 20%
Modulus Elastis 200 IPK 29x10^6 psi

Kirim permintaan