Pelat Baja Tahan Karat 316/316L – Paduan Tahan-Kinerja Tinggi-Tahan Karat

Mar 09, 2026

Tinggalkan pesan

What is 1.4565 Stainless Steel?What is 1.4523 Stainless Steel?What is 1.4537 Stainless Steel?

Ketebalan yang tersedia untuk Paduan 316/316L:

3/16" 1/4" 5/16" 3/8" 7/16" 1/2" 9/16" 5/8" 3/4" 7/8" 1" 1 1/8"
4.8mm 6.3mm 7.9mm 9.5mm 11.1mm 12.7mm 14.3mm 15.9mm 19mm 22.2mm 25.4mm 28.6mm
1 1/4" 1 3/8" 1 1/2" 1 5/8" 1 3/4" 2" 2 1/4" 2 1/2" 2 3/4" 3" 3 1/4" 3 1/2"
31.8mm 34.9mm 38.1mm 41.3mm 44.5mm 50.8mm 57.2mm 63.5mm 69.9mm 76.2mm 82.6mm 88.9mm
3 3/4" 4" 4 1/4" 4 1/2" 4 3/4" 5" 5 1/4" 5 1/2" 5 3/4" 6"    
95.3mm 101.6mm 108mm 114.3mm 120.7mm 127mm 133.4mm 139.7mm 146.1mm 152.4mm    

 

Analisis Kimia

% Bobot (semua nilai adalah maksimum kecuali rentangnya dinyatakan lain)

Elemen 316 316L
Kromium 16,0 menit-18,0 maks. 16,0 menit-18,0 maks.
Nikel 10,0 menit-14,0 maks. 10,0 menit-14,0 maks.
molibdenum 2,00 menit-3,00 maks. 2,00 menit-3,00 maks.
Karbon 0.08 0.030
mangan 2.00 2.00
Fosfor 0.045 0.045
belerang 0.03 0.03
Silikon 0.75 0.75
Nitrogen 0.1 0.1
Besi Keseimbangan Keseimbangan

 