420 Produk Baja Tahan Karat

Mar 23, 2026

Tinggalkan pesan

304 Stainless Steel Coil for Deep Drawing and Stamping304L Stainless Steel Pipe for Chemical Fluid Transportation304 Stainless Steel Sheet for Architectural Decoration

 

Komposisi Kimia

Elemen

C (Karbon)

Cr (Kromium)

Mn (Mangan)

Si (Silikon)

P (Fosfor)

S (Belerang)

Ni (Nikel)

Besi (Fe)

Besi (Fe)

Isi 0.15% – 0.40% 12.0% – 14.0% maks 1,0%. maks 1,0%. 0,04% maks 0,03% maks maks 0,75%. Keseimbangan \

Sifat Mekanik

Properti

Satuan Metrik

Satuan Kekaisaran

Kekuatan Tarik 655 – 860 MPa 95 – 125xi
Kekuatan Hasil 450MPa 65ksi
Kekerasan Vickers 230 – 270 HV 230 – 270 HV
Kekerasan Brinell 200 – 250 HB 200 – 250 HB
Kekerasan Rockwell 50 – 56 HRC 50 – 56 HRC
Pemanjangan 20% 20%
Modulus Elastis 200 IPK 29x10^6 psi